Penetration Grade

The use of penetrating bitumen is mainly in road construction.

For areas with hotter climates, harder bitumen (less penetration degree) is used, and for areas with colder climates, looser bitumen (higher penetration degree) is used.

Analyze

TestMethod30-4040-5060-7085-100100-120
DensityASTM D-706/1-01/106/1-01/106/1-01/15 0/1-104/1-01/1
Penetration ,25°c ASTM D-530-4040-5060-7085-100100-120
Softening point °CASTM D-3655-6352-6049-5645-5242-49
Ductility ,25°cASTM D-113Min 100Min 100Min 100Min 100Min 100
Flash Point °CASTM-D92250 min 250 min 250 min 250 min 250 min
Solubility in disulfide%wt. ASTM D-45/995/995/995/995/99
Spot test AASHTO T 102Negative Negative Negative Negative Negative
Loss on heating(%wt)Max 2 /0Max 2 /0Max 2 /0Max 2 /0Max 2 /0Max 2 /0
Drop in penetration after heating% ASTM D-6-D-520 Max20 Max20 Max20 Max20 Max